Research Data Data selection strategies for minimizing measurement time in materials characterization, measurement data(Universität Kassel) Liehr, Alexander; Dingel, Kristina; Degener, Sebastian; Kottke, Daniel; Meier, David; Niendorf, Thomas; Sick, BernhardEvery new material needs to be assessed and qualified for an envisaged application. A steadily increasing number of new alloys, designed to address challenges in terms of reliability and sustainability, poses significant demands on well-known analysis methods in terms of their efficiency, e.g., in X-Ray diffraction analysis. Particularly in laboratory measurements, where the intensities in diffraction experiments tend to be low, a possibility to adapt the exposure time to the prevailing boundary conditions, i.e., the investigated microstructure, is seen to be a very effective approach. The counting time is decisive for, e.g., complex texture, phase, and residual stress measurements. Traditionally, more measurement points and, thus, longer data collection times lead to more accurate information. Here, too short counting times result in poor signal-to-background ratios and dominant signal noise, respectively, rendering subsequent evaluation more difficult or even impossible. Then, it is necessary to repeat experiments with adjusted, usually significantly longer counting time. To prevent redundant measurements, it is state-of-the-art to always consider the entire measurement range, regardless of whether the investigated points are relevant and contribute to the subsequent materials characterization, respectively. Obviously, this kind of approach is extremely time consuming and, eventually, not efficient. All relevant data including the code are carefully assessed and will be the basis for a widely adapted strategy enabling efficient measurements not only in lab environments but also large scale facilities.
This data set consists of the fully measured data from the diffraction experiments as well as the manuscript for data analyzing.
IMPORTANT: In case you use the data please cite our corresponding article: https://doi.org/10.1038/s41598-025-96221-1Research Data Impact of a single-side 100Cr6 clad layer on the tensile and fatigue properties of S550MC steel [Dataset](Universität Kassel) Krochmal, Marcel; Wegener, Thomas; Niendorf, ThomasThe production of newly developed hot-rolled layered metal composites (LMC) leads to the availability of sheet materials with specifically adjustable, graded properties being cost-effective and suitable for large-scale production. As many of the envisaged applications of these LMC, e.g., clutch disc carriers, suffer from cyclic loading during service life, a fundamental knowledge of the fatigue behavior is required in order to ensure safe and reliable application of the components. Therefore, the study described in https://doi.org/10.1111/ffe.14383 focuses on the fatigue behavior of a hot-rolled two-layer LMC consisting of a S550MC substrate layer and a 100Cr6 clad layer. In order to investigate the influence of the clad layer, two conditions are directly compared, i.e., the two-layer laminate cladded steel and the single-layer substrate condition.Research Data Source code for a program to calculate Schmid-factorsFrenck, Johanna-Maria; Frenck, Georg; Degener, Sebastian; Vollmer, Malte; Niendorf, ThomasResearch Data Surface layer state after hard turning of 51CrV4(Universität Kassel) Wittich, Felix; Wegener, Thomas; Liehr, Alexander; Zinn, Wolfgang; Niendorf, Thomas; Kroll, AndreasDescription of the dataset:
Hard-turning experiments were conducted on cylindrical specimens made of a quenched and tempered (Q&T) steel 51CrV4
in different initial surface hardness levels, i. e. 400 HV30, 500 HV30 and 600 HV30. Prior to heat treatment,
all specimens were manufactured with the same roughness requirements in order to ensure an almost identical surface
finish before hard-turning. Three different sections of nine specimen of each hardness level
(i.e. in total 27 section-specific areas per hardness level) were machined with varied cutting parameters feed rate
(f), depth of cut (a_p) and cutting speed (v_c).
Hard-turning of the specimens was carried out on a servo-conventional lathe of type Weiler C30 using
polycrystalline boron nitride (PCBN) inserts with a corner radius of 0.8 mm.
After hard-turning, residual stress depth profiles were determined using X-ray diffraction (XRD),
respectively for each specific area of a specimen. Residual stress measurements were conducted using a
Pulstec μ-X360 diffractometer equipped with a 0.3 mm collimator and CrKα-radiation with an exposure time
of 120 sec. Depth profiles were determined by successive removal of the material surface layer using
electro-chemical polishing. The obtained data have been evaluated applying the cos α-method without consideration
of any mathematical stress correction.
Post process surface roughness in axial direction was determined using a Mitutoyo SJ-210 tactile roughness
measuring device. Post process Vickers hardness testing was carried out using a Struers DuraScan-70 system
employing a load of 294.2 N (HV30).
For more detailed information on the material and the experimental setup, i.e., chemical composition, specimen
geometry, machines and parameters used for hard-turning operations and post process measurements, the reader is
referred to [1].
A full factorial experiment design was used with two levels for the initial hardness levels H_Vinit and three
factors for the cutting parameters, f: {0.05 mm, 0.25 mm, 0.5 mm}, v_c: {100 m/min, 175 m/min, 250 m/min},
a_p: {0.05 mm, 0.25 mm, 0.5 mm}, resulting in 81 different combinations. For the residual stress depth profile
modeling, measurements for 12 different depths are available:
{0, 10, 20, 30, 40, 50, 60, 80, 100, 120, 150, 200} μm, providing for N = 972 samples in total.
Two data sets are provided:
1. "hardness_roughness_hard_turning.csv" with the 81 data points for the surface hardness and roughness measurements.
2. "residual_stress_profile_hard_turning.csv" with the 972 data points for the tangential residual stress depth profiles.
[1] Thomas Wegener, Alexander Liehr, Artjom Bolender, Sebastian Degener, Felix Wittich, Andreas Kroll, & Thomas Niendorf,
"Calibration and validation of micromagnetic data for non-destructive analysis of near-surface properties
after hard turning" in HTM Journal of Heat Treatment and Materials, 2022, 77(2), 156-172.